Nanoindentation mapping of mechanical properties of cement paste and natural rocks
- Wenzhong Zhu
- , John J, Hughes
- , Nenad Bicanic
- , Chris J. Pearce
Research output: Contribution to journal › Article › peer-review
231
Link opens in a new tab
Citations
(Scopus)